High Performance Water Reducer Polycarboxylate Superplasticizer Liquid 40% 50% Solid Content
Contact Person : Jack
Phone Number : 0086-13955140199
WhatsApp : +8613955140199
Minimum Order Quantity : | 1Tons | Price : | Negotiation |
---|---|---|---|
Packaging Details : | 25kgs/Bag,16Tons/20'gp | Delivery Time : | Within 15 days after order confirmation |
Payment Terms : | T/T, L/C, D/A, D/P, | Supply Ability : | 900000TONS/YEAR |
Place of Origin: | China | Brand Name: | ELITE-INDUS |
---|---|---|---|
Certification: | ISO | Model Number: | Elt-NSF |
Detail Information |
|||
Appearance: | Light Brown Powder | Sodium Sulphate Content: | 5% Or 10% Or 19% |
---|---|---|---|
PH Value: | 7-9 | Surface Tension: | 70±1×10-3N/M |
Surface Tension(N/m): | (7 1 ± 1) ×10-3 | Product Name: | Water Reducer Concrete Additives Sodium Naphthalene Sulfonate Formaldehyde SNF PNS |
High Light: | polycarboxylate concrete admixtures,concrete water reducer |
Product Description
Concrete water reducer sodium naphthalene sulfonic formaldehyde SNF PNS FDN
------Elt-NSF
1. SNF Introduction
Naphthalene formaldehyde sulphonate water reducing agent
is a synthetic powder based on beta-sulphonate formaldehyde Condensate and reactive polymer.
It has the properties of high range water reduction, set retarding and excellent strengthening.
Elt-nsf sodium sulfate is less than 10% , suitable to middle strength or high strength
concrete where high range water reduction is desired.
2. SNF Specification
INDEX ITEM | Elt-A | Elt-B | Elt-C |
Appearance | Light brown powder | Light brown powder | Light brown powder |
Solid Content | ≥ 92 | ≥ 92 | ≥ 92 |
Sodium sulphate Content | 5% | 10% | 20% |
Chloride Content | 0.3% | 0.4% | 0.5% |
PH Value | 7-9 | 7-9 | 7-9 |
Net Starch Fluidity | ≥ 250 mm | ≥ 240 mm | ≥ 230 mm |
Surface Tension | 70±1×10-3N/M | 70±1×10-3N/M | 70±1×10-3N/M |
3. SNF Package
25kgs/Bag or Ton bag,16Tons/20'gp
4. SNF Application
A. Used for and widely for self-cured, vapor-cured concrete and its formulations.
At the early stage of application, extremely prominent effects are shown.
As the result, the modulus and site utilization can be drastically, the procedure of vapor cure is omitted in peak-heat summer days.
Statistically 40-60 metric tons of coal will be preserved when a metric ton of the material is consumed.
B. Suitable for preparation of early-strength, high-strength, high-anti-filtration and self-sealing& pumpable concrete.
C. Widely used in pre-cast & ready-mixed concrete, armored concrete and pre-stressed reinforced concrete in key construction projects
such as dam and port construction, road building & town planning projects and dwelling erections etc.
D. Compatible with Portland cement, normal Portland cement,
Portland slag cement, fly-ash cement and Portland pozzolanic cement etc.
5. SNF USAGE:
A. Blending dosage at 0.5%-1.0%, 0.6% mixing dosage advised.
B. Prepare solutions as required.
C. Direct use of powder agent is allowed.
Alternatively the addition of the agent is followed by water moisturization (water-cement ratio: 60%).
6. Parameters & accepttance criteria (For reference)
A. Elt-A
Parameters | Criteria | Actual Results | Parammeters | Criteria | Actual Results | ||
Water reduction, Min % |
≥14 | 18-28 | Compression strength,% | 1d | ≥140 | 170 | |
Water Penetration, Max % |
≤ 90 | 79 | 3d | ≥130 | 160 | ||
Air Content,% | ≤ 3.0 | 1.6 | 7d | ≥125 | 145 | ||
Temporal distribution for setting (min) | Initial setting time | -90 ~ +120 |
|
28d | ≥120 | 135 | |
Terminal setting time | Shrinkage,% |
|
|
|
|||
Corrosion to steel bars | None | None | |||||
Note:Standard Blend Dosage: 0.75% (as cement amount) |
B. Elt-B
Parameters | Criteria | Actual Results | Parammeters | Criteria | Actual Results | ||
Water reduction, Min % | ≥14 | 17-25 | Compression strength,% | 1d | ≥140 | 165 | |
Water Penetration, Max % | ≤90 | 80 | 3d | ≥130 | 155 | ||
Air Content, % | ≤3.0 | 1.6 | 7d | ≥125 | 140 | ||
Temporal distribution for setting(min) | Initial setting time | -90 ~ +120 |
|
28d | ≥120 | 130 | |
Terminal setting time | Shrinkage,% |
|
|
|
|||
Corrosion to steel bars | None | None | |||||
Note:Standard Blend Dosage: 0.75% (as cement amount) |
C. Elt-C
Parameters | Criteria | Actual Results | Parammeters | Criteria | Actual Results | ||
Water reduction,Min % | ≥14 | 16-22 | Compression strength,% | 1d | ≥140 | 160 | |
Water Penetration,Max % | ≤90 | 85 | 3d | ≥130 | 150 | ||
Air Content,% | ≤3.0 | 2.0 | 7d | ≥125 | 140 | ||
Temporal distribution for setting(min) | Initial setting time | -90 ~ +120 |
|
28d | ≥120 | 125 | |
Terminal setting time | Shrinkage,% |
|
|
|
|||
Corrosion to steel bars | None | None | |||||
Note:Standard Blend Dosage: 0.75% (as cement amount) |